Wood Record

genus

Morus

Woods sold under several trade names often come from one genus. These 5 share the genus Morus, so they are close relatives and frequent substitutes for each other.

0 of 5 carry a published Janka test.

WoodJankaDensity
Black mulberryMorus nigra1,152 lbf*41.3 lb/ft³
DifouMorus mesozygia2,139 lbf*54.0 lb/ft³
Red mulberryMorus rubra1,152 lbf*41.3 lb/ft³
Texas mulberryMorus microphylla1,598 lbf*48.1 lb/ft³
White mulberryMorus alba1,363 lbf*44.7 lb/ft³