Wood Record

genus

Myrsine

Woods sold under several trade names often come from one genus. These 4 share the genus Myrsine, so they are close relatives and frequent substitutes for each other.

0 of 4 carry a published Janka test.

WoodJankaDensity
Kokea lau liiMyrsine sandwicensis1,255 lbf*43.0 lb/ft³
Kolea lau nuiMyrsine lessertiana1,203 lbf*42.1 lb/ft³
Lanai colicwoodMyrsine lanaiensis1,538 lbf*47.3 lb/ft³
Leathery colicwoodMyrsine coriacea1,363 lbf*44.7 lb/ft³