genus
Nectandra
Woods sold under several trade names often come from one genus. These 5 share the genus Nectandra, so they are close relatives and frequent substitutes for each other.
1 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Canela/louro-tamancoNectandra cuspidata | 573 lbf* | 28.7 lb/ft³ |
| CaneloNectandra spp. | 1,060 lbf | 39.0 lb/ft³ |
| Nectandra membranaceaNectandra membranacea | 875 lbf* | 36.3 lb/ft³ |
| Nectandra turbacensisNectandra turbacensis | 1,103 lbf* | 40.5 lb/ft³ |
| ShinglewoodNectandra hihua | 679 lbf* | 32.3 lb/ft³ |