Wood Record

genus

Nyssa

Woods sold under several trade names often come from one genus. These 4 share the genus Nyssa, so they are close relatives and frequent substitutes for each other.

2 of 4 carry a published Janka test.

WoodJankaDensity
Black tupeloNyssa sylvatica810 lbf35.0 lb/ft³
Ogeechee tupeloNyssa ogeche791 lbf*34.7 lb/ft³
Swamp tupeloNyssa biflora791 lbf*34.7 lb/ft³
Water tupeloNyssa aquatica880 lbf35.0 lb/ft³