genus
Ocotea
Woods sold under several trade names often come from one genus. These 12 share the genus Ocotea, so they are close relatives and frequent substitutes for each other.
8 of 12 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AbacatiranaOcotea aciphylla = Ocotea costulata | 1,025 lbf | 38.7 lb/ft³ |
| Demerara GreenheartOcotea rodiaei | 2,360 lbf | 66.0 lb/ft³ |
| DetermaOcotea rubra | 660 lbf | 42.0 lb/ft³ |
| East African CamphorwoodOcotea usambarensis | 930 lbf | 37.0 lb/ft³ |
| Laurel espadaOcotea floribunda | 753 lbf* | 33.9 lb/ft³ |
| Loblolly sweetwoodOcotea leucoxylon | 915 lbf* | 37.1 lb/ft³ |
| LouroOcotea sp. | 1,198 lbf | 38.4 lb/ft³ |
| Louro-mamorimOcotea cymbarum = Ocotea barcellensis | 1,135 lbf | 42.1 lb/ft³ |
| Louro-pretoOcotea neesiana | 1,010 lbf | 42.1 lb/ft³ |
| Louro-pretoOcotea fragrantissima | 1,063 lbf | 36.2 lb/ft³ |
| NemocaOcotea moschata | 1,419 lbf* | 45.5 lb/ft³ |
| Nemoca cimarronaOcotea spathulata | 1,419 lbf* | 45.5 lb/ft³ |