Woods sold under several trade names often come from one genus. These 2 share the genus Olea, so they are close relatives and frequent substitutes for each other.

1 of 2 carry a published Janka test.

WoodJankaDensity
East African OliveOlea hochstetteri2,740 lbf55.0 lb/ft³
OliveOlea europaea3,336 lbf*67.7 lb/ft³