Wood Record

genus

Ormosia

Woods sold under several trade names often come from one genus. These 5 share the genus Ormosia, so they are close relatives and frequent substitutes for each other.

3 of 5 carry a published Janka test.

WoodJankaDensity
BaracaraOrmosia spp.1,000 lbf44.0 lb/ft³
ChedebsungelOrmosia calavensis1,054 lbf*39.6 lb/ft³
PeroniaOrmosia krugii753 lbf*33.9 lb/ft³
TentoOrmosia paraensis1,688 lbf45.6 lb/ft³
TentoOrmosia coccinea1,378 lbf44.9 lb/ft³