genus
Oxandra
Woods sold under several trade names often come from one genus. These 2 share the genus Oxandra, so they are close relatives and frequent substitutes for each other.
1 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| HayaOxandra laurifolia | 1,725 lbf* | 49.9 lb/ft³ |
| West Indian LancewoodOxandra lanceolata | 2,830 lbf | 62.0 lb/ft³ |