genus
Palicourea
Woods sold under several trade names often come from one genus. These 3 share the genus Palicourea, so they are close relatives and frequent substitutes for each other.
0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Palicourea croceoidesPalicourea croceoides | 875 lbf* | 36.3 lb/ft³ |
| Red cappelPalicourea crocea | 1,054 lbf* | 39.6 lb/ft³ |
| Showy cappelPalicourea guianensis | 753 lbf* | 33.9 lb/ft³ |