Wood Record

genus

Parinari

Woods sold under several trade names often come from one genus. These 3 share the genus Parinari, so they are close relatives and frequent substitutes for each other.

2 of 3 carry a published Janka test.

WoodJankaDensity
BuradaParinari spp.1,830 lbf52.0 lb/ft³
Parinari / bafo-de-boi-mirimParinari excelsa2,522 lbf57.4 lb/ft³
SeaParinari insularum1,852 lbf*51.5 lb/ft³