genus
Parkia
Woods sold under several trade names often come from one genus. These 7 share the genus Parkia, so they are close relatives and frequent substitutes for each other.
5 of 7 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Fava-bolota / visgueiroParkia gigantocarpa | 463 lbf | 19.4 lb/ft³ |
| FaveiraParkia nitida = Parkia oppositifolia | 621 lbf | 27.5 lb/ft³ |
| FaveiraParkia multijuga | 668 lbf | 28.2 lb/ft³ |
| Faveira / visgueiroParkia paraensis | 743 lbf | 33.1 lb/ft³ |
| Parkia timorianaParkia timoriana | 608 lbf* | 30.7 lb/ft³ |
| RoxinhoParkia sp | 276 lbf* | 20.0 lb/ft³ |
| RoxinhoParkia pendula | 952 lbf | 38.4 lb/ft³ |