Woods sold under several trade names often come from one genus. These 3 share the genus Peltogyne, so they are close relatives and frequent substitutes for each other.

3 of 3 carry a published Janka test.

WoodJankaDensity
AngicoPeltogyne cf subsessilis2,941 lbf60.6 lb/ft³
PurpleheartPeltogyne spp.1,860 lbf58.0 lb/ft³
RosadinhoPeltogyne paniculata3,386 lbf64.3 lb/ft³