WoodJankaDensity
AvocadoPersea americana791 lbf*34.7 lb/ft³
LinguePersea spp.860 lbf36.0 lb/ft³
RedbayPersea borbonia1,007 lbf*38.8 lb/ft³
Swamp bayPersea palustris1,152 lbf*41.3 lb/ft³