genus

Pimenta

Woods sold under several trade names often come from one genus. These 2 share the genus Pimenta, so they are close relatives and frequent substitutes for each other.

0 of 2 carry a published Janka test.

WoodJankaDensity
AllspicePimenta dioica3,441 lbf*68.7 lb/ft³
BayrumtreePimenta racemosa3,147 lbf*65.9 lb/ft³