genus
Pinus
Woods sold under several trade names often come from one genus. These 57 share the genus Pinus, so they are close relatives and frequent substitutes for each other.
17 of 57 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Aleppo pinePinus halepensis | 599 lbf* | 32.3 lb/ft³ |
| Apache pinePinus engelmannii | 599 lbf* | 32.3 lb/ft³ |
| Arizona pinePinus arizonica | 599 lbf* | 32.3 lb/ft³ |
| Austrian pinePinus nigra | 599 lbf* | 32.3 lb/ft³ |
| Benguet PinePinus insularis | 605 lbf | 35.0 lb/ft³ |
| Bishop pinePinus muricata | 645 lbf* | 33.9 lb/ft³ |
| Border pinyonPinus discolor | 599 lbf* | 32.3 lb/ft³ |
| Bunge's pinePinus bungeana | 599 lbf* | 32.3 lb/ft³ |
| Canary Island pinePinus canariensis | 599 lbf* | 32.3 lb/ft³ |
| Caribbean pinePinus caribaea | 1,240 lbf | 38.0 lb/ft³ |
| Chihuahuan pinePinus leiophylla | 599 lbf* | 32.3 lb/ft³ |
| Chinese red pinePinus massoniana | 740 lbf* | 37.1 lb/ft³ |
| Common or two-needle pinyonPinus edulis | 766 lbf* | 38.0 lb/ft³ |
| Coulter pinePinus coulteri | 599 lbf* | 32.3 lb/ft³ |
| Eastern white pinePinus strobus | 380 lbf | 24.5 lb/ft³ |
| Five-needle pinePinus parviflora | 599 lbf* | 32.3 lb/ft³ |
| Four-leaf or Parry pinyon pinePinus quadrifolia | 599 lbf* | 32.3 lb/ft³ |
| Foxtail pinePinus balfouriana | 599 lbf* | 32.3 lb/ft³ |
| Gray or California foothill pinePinus sabiniana | 532 lbf* | 29.8 lb/ft³ |
| Great Basin bristlecone pinePinus longaeva | 599 lbf* | 32.3 lb/ft³ |
| Indian longleaf pinePinus roxburghii | 668 lbf* | 34.7 lb/ft³ |
| Italian stone pinePinus pinea | 599 lbf* | 32.3 lb/ft³ |
| Jack pinePinus banksiana | 570 lbf | 30.1 lb/ft³ |
| Japanese black pinePinus thunbergii | 599 lbf* | 32.3 lb/ft³ |
| Japanese red pinePinus densiflora | 599 lbf* | 32.3 lb/ft³ |
| Jeffrey pinePinus jeffreyi | 469 lbf* | 27.5 lb/ft³ |
| Knobcone pinePinus attenuata | 511 lbf* | 29.1 lb/ft³ |
| Limber pinePinus flexilis | 469 lbf* | 27.5 lb/ft³ |
| Loblolly pinePinus taeda | 690 lbf | 35.6 lb/ft³ |
| Lodgepole pinePinus contorta | 480 lbf | 28.7 lb/ft³ |
| Longleaf pinePinus palustris | 870 lbf | 41.3 lb/ft³ |
| Maritime pinePinus pinaster | 766 lbf* | 38.0 lb/ft³ |
| Merkus PinePinus merkusii | 620 lbf | 43.0 lb/ft³ |
| Mexican pinyon pinePinus cembroides | 599 lbf* | 32.3 lb/ft³ |
| Ocote pinePinus oocarpa | 910 lbf | 41.0 lb/ft³ |
| Papershell pinyon pinePinus remota | 599 lbf* | 32.3 lb/ft³ |
| Patula PinePinus patula (plantation) | 645 lbf* | 34.0 lb/ft³ |
| Pitch pinePinus rigida | 717 lbf* | 36.3 lb/ft³ |
| Pond pinePinus serotina | 803 lbf* | 39.1 lb/ft³ |
| Ponderosa pinePinus ponderosa | 460 lbf | 28.0 lb/ft³ |
| Radiata pinePinus radiata | 750 lbf | 31.5 lb/ft³ |
| Red pinePinus resinosa | 560 lbf | 32.2 lb/ft³ |
| Rocky Mountain bristlecone pinePinus aristata | 599 lbf* | 32.3 lb/ft³ |
| Sand pinePinus clausa | 635 lbf* | 33.6 lb/ft³ |
| Scots pinePinus sylvestris | 621 lbf* | 33.1 lb/ft³ |
| Shortleaf pinePinus echinata | 690 lbf | 35.6 lb/ft³ |
| Singleleaf pinyonPinus monophylla | 599 lbf* | 32.3 lb/ft³ |
| Slash pinePinus elliottii | 869 lbf* | 41.3 lb/ft³ |
| Southwestern white pinePinus strobiformis | 599 lbf* | 32.3 lb/ft³ |
| Spruce pinePinus glabra | 660 lbf | 30.8 lb/ft³ |
| Sugar pinePinus lambertiana | 380 lbf | 25.2 lb/ft³ |
| Table Mountain pinePinus pungens | 740 lbf* | 37.1 lb/ft³ |
| Torrey pinePinus torreyana | 599 lbf* | 32.3 lb/ft³ |
| Virginia pinePinus virginiana | 740 lbf | 33.6 lb/ft³ |
| Washoe pinePinus washoensis | 599 lbf* | 32.3 lb/ft³ |
| Western white pinePinus monticola | 420 lbf | 26.6 lb/ft³ |
| Whitebark pinePinus albicaulis | 599 lbf* | 32.3 lb/ft³ |