Wood Record

genus

Piper

Woods sold under several trade names often come from one genus. These 5 share the genus Piper, so they are close relatives and frequent substitutes for each other.

0 of 5 carry a published Janka test.

WoodJankaDensity
Guyanese pepperPiper glabrescens423 lbf*26.0 lb/ft³
Higuillo de hoja menudaPiper aduncum573 lbf*29.8 lb/ft³
Higuillo de limonPiper amalago1,152 lbf*41.3 lb/ft³
Jamaican pepperPiper hispidum714 lbf*33.1 lb/ft³
Moth pepperPiper blattarum714 lbf*33.1 lb/ft³