Wood Record

genus

Pittosporum

Woods sold under several trade names often come from one genus. These 6 share the genus Pittosporum, so they are close relatives and frequent substitutes for each other.

0 of 6 carry a published Janka test.

WoodJankaDensity
Australian cheesewoodPittosporum undulatum1,788 lbf*50.7 lb/ft³
Cape cheesewoodPittosporum viridiflorum1,309 lbf*43.8 lb/ft³
Cream cheesewoodPittosporum terminalioides1,598 lbf*48.1 lb/ft³
Japanese cheesewoodPittosporum tobira1,788 lbf*50.7 lb/ft³
KamalPittosporum ferrugineum1,419 lbf*45.5 lb/ft³
Taiwanese cheesewoodPittosporum pentandrum1,203 lbf*42.1 lb/ft³