Woods sold under several trade names often come from one genus. These 6 share the genus Platanus, so they are close relatives and frequent substitutes for each other.

1 of 6 carry a published Janka test.

WoodJankaDensity
American sycamorePlatanus occidentalis770 lbf34.3 lb/ft³
Arizona sycamorePlatanus wrightii791 lbf*34.7 lb/ft³
California sycamorePlatanus racemosa791 lbf*34.7 lb/ft³
London planetreePlatanus hybrida791 lbf*34.7 lb/ft³
Mexican sycamorePlatanus mexicana791 lbf*34.7 lb/ft³
Oriental planetreePlatanus orientalis791 lbf*34.7 lb/ft³