Podocarpus
Woods sold under several trade names often come from one genus. These 5 share the genus Podocarpus, so they are close relatives and frequent substitutes for each other.
3 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| PodoPodocarpus spp. | 830 lbf | 32.0 lb/ft³ |
| PodocarpPodocarpus spp. | 760 lbf | 35.0 lb/ft³ |
| TotaraPodocarpus spp. | 655 lbf | 32.0 lb/ft³ |
| Yew plum pinePodocarpus macrophyllus | 898 lbf* | 42.1 lb/ft³ |
| Yucca plum pinePodocarpus coriaceus | 1,255 lbf* | 43.0 lb/ft³ |