Woods sold under several trade names often come from one genus. These 10 share the genus Populus, so they are close relatives and frequent substitutes for each other.

3 of 10 carry a published Janka test.

WoodJankaDensity
Balsam poplarPopulus balsamifera351 lbf*23.8 lb/ft³
Bigtooth aspenPopulus grandidentata471 lbf*27.3 lb/ft³
Black cottonwoodPopulus balsamifera ssp. trichocarpa350 lbf24.5 lb/ft³
Black poplarPopulus nigra509 lbf*28.2 lb/ft³
Eastern cottonwoodPopulus deltoides430 lbf28.0 lb/ft³
Fremont cottonwoodPopulus fremontii608 lbf*30.7 lb/ft³
Narrowleaf cottonwoodPopulus angustifolia423 lbf*26.0 lb/ft³
Quaking aspenPopulus tremuloides350 lbf26.6 lb/ft³
Silver poplarPopulus alba423 lbf*26.0 lb/ft³
Swamp cottonwoodPopulus heterophylla423 lbf*26.0 lb/ft³