genus
Pouteria
Woods sold under several trade names often come from one genus. These 12 share the genus Pouteria, so they are close relatives and frequent substitutes for each other.
8 of 12 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Abiu-brancoPouteria oppositifolia | 1,788 lbf* | 50.7 lb/ft³ |
| AbiuranaPouteria anomala | 2,472 lbf | 56.2 lb/ft³ |
| AbiuranaPouteria sp | 2,418 lbf | 57.4 lb/ft³ |
| AbiuranaPouteria egregia | 2,950 lbf | 67.7 lb/ft³ |
| AbiuranaPouteria guianensis | 2,921 lbf | 58.7 lb/ft³ |
| Abiurana-brancaPouteria caimito | 2,608 lbf | 56.8 lb/ft³ |
| BullytreePouteria multiflora | 2,064 lbf* | 54.2 lb/ft³ |
| EggfruitPouteria campechiana | 2,448 lbf* | 58.7 lb/ft³ |
| Mammee sapotePouteria sapota | 1,923 lbf* | 52.4 lb/ft³ |
| MaragonçaloPouteria obscura | 1,746 lbf | 48.7 lb/ft³ |
| TuturubáPouteria gongrijpii = Franchetella gongrijpii | 2,396 lbf | 56.9 lb/ft³ |
| TuturubáPouteria oblanceolata | 2,923 lbf | 59.9 lb/ft³ |