genus
Prosopis
Woods sold under several trade names often come from one genus. These 4 share the genus Prosopis, so they are close relatives and frequent substitutes for each other.
0 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Honey mesquiteProsopis glandulosa | 2,779 lbf* | 62.2 lb/ft³ |
| JandProsopis cineraria | 1,538 lbf* | 47.3 lb/ft³ |
| Screwbean mesquiteProsopis pubescens | 2,779 lbf* | 62.2 lb/ft³ |
| Velvet mesquiteProsopis velutina | 2,779 lbf* | 62.2 lb/ft³ |