Wood Record

genus

Protium

Woods sold under several trade names often come from one genus. These 3 share the genus Protium, so they are close relatives and frequent substitutes for each other.

3 of 3 carry a published Janka test.

WoodJankaDensity
BreuProtium sp.2,317 lbf39.0 lb/ft³
BreuProtium heptaphyllum877 lbf42.1 lb/ft³
Breu-pretoProtium tenuifolium1,517 lbf48.9 lb/ft³