genus
Prunus
Woods sold under several trade names often come from one genus. These 24 share the genus Prunus, so they are close relatives and frequent substitutes for each other.
1 of 24 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Allegheny plumPrunus alleghaniensis | 832 lbf* | 35.5 lb/ft³ |
| American plumPrunus americana | 832 lbf* | 35.5 lb/ft³ |
| ApricotPrunus armeniaca | 1,725 lbf* | 49.9 lb/ft³ |
| Bitter cherryPrunus emarginata | 832 lbf* | 35.5 lb/ft³ |
| Black cherryPrunus serotina | 950 lbf | 35.0 lb/ft³ |
| Canada plumPrunus nigra | 832 lbf* | 35.5 lb/ft³ |
| Carolina laurelcherryPrunus caroliniana | 832 lbf* | 35.5 lb/ft³ |
| Cherry laurelPrunus laurocerasus | 875 lbf* | 36.3 lb/ft³ |
| Cherry plumPrunus cerasifera | 832 lbf* | 35.5 lb/ft³ |
| Chickasaw plumPrunus angustifolia | 832 lbf* | 35.5 lb/ft³ |
| ChokecherryPrunus virginiana | 832 lbf* | 35.5 lb/ft³ |
| European plumPrunus domestica | 832 lbf* | 35.5 lb/ft³ |
| Japanese flowering cherryPrunus serrulata | 832 lbf* | 35.5 lb/ft³ |
| Japanese plumPrunus salicina | 832 lbf* | 35.5 lb/ft³ |
| Mahaleb cherryPrunus mahaleb | 832 lbf* | 35.5 lb/ft³ |
| Mexican plumPrunus mexicana | 832 lbf* | 35.5 lb/ft³ |
| PeachPrunus persica | 832 lbf* | 35.5 lb/ft³ |
| Pin cherryPrunus pensylvanica | 832 lbf* | 35.5 lb/ft³ |
| Sargent cherryPrunus sargentii | 832 lbf* | 35.5 lb/ft³ |
| Sour cherryPrunus cerasus | 832 lbf* | 35.5 lb/ft³ |
| Sweet almondPrunus dulcis | 832 lbf* | 35.5 lb/ft³ |
| West Indian cherryPrunus myrtifolia | 1,923 lbf* | 52.4 lb/ft³ |
| Western cherry laurelPrunus occidentalis | 2,287 lbf* | 56.9 lb/ft³ |
| Wild cherryPrunus avium | 1,152 lbf* | 41.3 lb/ft³ |