Wood Record

genus

Pterocarpus

Woods sold under several trade names often come from one genus. These 8 share the genus Pterocarpus, so they are close relatives and frequent substitutes for each other.

5 of 8 carry a published Janka test.

WoodJankaDensity
African PadaukPterocarpus soyauxii1,538 lbf*46.0 lb/ft³
Andaman PadaukPterocarpus dalbergioides1,630 lbf48.9 lb/ft³
Burma PadaukPterocarpus macrocarpus2,170 lbf54.0 lb/ft³
Dragonsblood treePterocarpus officinalis875 lbf*36.3 lb/ft³
Embira-de-preguiçaPterocarpus sp.1,731 lbf33.0 lb/ft³
Malabar kinoPterocarpus marsupium2,210 lbf*55.9 lb/ft³
MuningaPterocarpus angolensis1,480 lbf41.0 lb/ft³
NarraPterocarpus indicus1,202 lbf40.0 lb/ft³