genus
Qualea
Woods sold under several trade names often come from one genus. These 3 share the genus Qualea, so they are close relatives and frequent substitutes for each other.
2 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| MandioqueiraQualea gracilior = Qualea cf lancifolia | 1,071 lbf | 44.7 lb/ft³ |
| MandioqueiraQualea brevipedicellata | 2,165 lbf | 58.7 lb/ft³ |
| Mandioqueira-escamosaQualea dinizii | 1,363 lbf* | 44.7 lb/ft³ |