17 of 72 carry a published Janka test.

WoodJankaDensity
Arizona white oakQuercus arizonica1,419 lbf*45.5 lb/ft³
Arkansas oakQuercus arkansana1,419 lbf*45.5 lb/ft³
Bastard oakQuercus sinuata1,475 lbf*46.4 lb/ft³
Bastard white oakQuercus austrina2,210 lbf*55.9 lb/ft³
Black oakQuercus velutina1,210 lbf42.6 lb/ft³
Blackjack oakQuercus marilandica1,419 lbf*45.5 lb/ft³
Blue oakQuercus douglasii1,419 lbf*45.5 lb/ft³
Bluejack oakQuercus incana1,419 lbf*45.5 lb/ft³
Buckley oakQuercus buckleyi1,419 lbf*45.5 lb/ft³
Bur oakQuercus macrocarpa1,370 lbf44.8 lb/ft³
California black oakQuercus kelloggii1,007 lbf*38.8 lb/ft³
California live oakQuercus agrifolia1,419 lbf*45.5 lb/ft³
California white oakQuercus lobata1,203 lbf*42.1 lb/ft³
Canyon live oakQuercus chrysolepis2,139 lbf*55.1 lb/ft³
Cherrybark oakQuercus pagoda1,480 lbf47.6 lb/ft³
Chestnut oakQuercus prinus1,130 lbf46.1 lb/ft³
Chinkapin oakQuercus muehlenbergii1,419 lbf*45.5 lb/ft³
Chisos oakQuercus graciliformis1,419 lbf*45.5 lb/ft³
Cork oakQuercus suber2,287 lbf*56.9 lb/ft³
Darlington oakQuercus hemisphaerica1,419 lbf*45.5 lb/ft³
Delta post oakQuercus similis1,419 lbf*45.5 lb/ft³
Durmast oakQuercus petraea1,419 lbf*45.5 lb/ft³
Dwarf chinkapin oakQuercus prinoides1,419 lbf*45.5 lb/ft³
Dwarf live oakQuercus minima1,419 lbf*45.5 lb/ft³
Dwarf post oakQuercus margarettiae1,419 lbf*45.5 lb/ft³
Emory oakQuercus emoryi1,419 lbf*45.5 lb/ft³
Engelmann oakQuercus engelmannii1,419 lbf*45.5 lb/ft³
European oakQuercus robur1,309 lbf*43.8 lb/ft³
European turkey oakQuercus cerris1,419 lbf*45.5 lb/ft³
Gambel oakQuercus gambelii1,538 lbf*47.3 lb/ft³
Graves oakQuercus gravesii1,419 lbf*45.5 lb/ft³
Gray oakQuercus grisea1,419 lbf*45.5 lb/ft³
Havard oakQuercus havardii1,419 lbf*45.5 lb/ft³
Holly oakQuercus ilex1,419 lbf*45.5 lb/ft³
Interior live oakQuercus wislizeni1,419 lbf*45.5 lb/ft³
Lacey oakQuercus laceyi1,419 lbf*45.5 lb/ft³
Lateleaf oakQuercus tardifolia1,419 lbf*45.5 lb/ft³
Laurel oakQuercus laurifolia1,210 lbf44.1 lb/ft³
Live oakQuercus virginiana2,712 lbf*61.6 lb/ft³
Mexican blue oakQuercus oblongifolia1,419 lbf*45.5 lb/ft³
Mexican white oakQuercus polymorpha1,419 lbf*45.5 lb/ft³
Myrtle oakQuercus myrtifolia1,419 lbf*45.5 lb/ft³
Netleaf oakQuercus rugosa1,419 lbf*45.5 lb/ft³
Northern pin oakQuercus ellipsoidalis1,419 lbf*45.5 lb/ft³
Northern red oakQuercus rubra1,290 lbf44.1 lb/ft³
Nuttall oakQuercus texana1,419 lbf*45.5 lb/ft³
OakQuercus spp.2,500 lbf53.0 lb/ft³
Oglethorpe oakQuercus oglethorpensis1,419 lbf*45.5 lb/ft³
Oregon white oakQuercus garryana1,725 lbf*49.9 lb/ft³
Overcup oakQuercus lyrata1,190 lbf44.1 lb/ft³
Pin oakQuercus palustris1,510 lbf44.1 lb/ft³
Post oakQuercus stellata1,360 lbf46.8 lb/ft³
Pungent oakQuercus pungens1,419 lbf*45.5 lb/ft³
Robust oakQuercus robusta1,419 lbf*45.5 lb/ft³
Sand live oakQuercus geminata1,419 lbf*45.5 lb/ft³
Sandpaper oakQuercus vaseyana1,419 lbf*45.5 lb/ft³
Sawtooth oakQuercus acutissima1,419 lbf*45.5 lb/ft³
Scarlet oakQuercus coccinea1,400 lbf46.8 lb/ft³
Scrub oakQuercus ilicifolia1,419 lbf*45.5 lb/ft³
Shingle oakQuercus imbricaria1,419 lbf*45.5 lb/ft³
Shumard oakQuercus shumardii1,419 lbf*45.5 lb/ft³
Silverleaf oakQuercus hypoleucoides1,419 lbf*45.5 lb/ft³
Sonoran scrub oakQuercus turbinella1,419 lbf*45.5 lb/ft³
Southern red oakQuercus falcata1,060 lbf41.3 lb/ft³
Swamp chestnut oakQuercus michauxii1,240 lbf46.8 lb/ft³
Swamp white oakQuercus bicolor1,620 lbf50.3 lb/ft³
Texas live oakQuercus fusiformis1,475 lbf*46.4 lb/ft³
Toumey oakQuercus toumeyi1,419 lbf*45.5 lb/ft³
Turkey oakQuercus laevis1,419 lbf*45.5 lb/ft³
Water oakQuercus nigra1,190 lbf44.1 lb/ft³
White oakQuercus alba1,360 lbf47.6 lb/ft³
Willow oakQuercus phellos1,460 lbf48.3 lb/ft³