Wood Record

genus

Rhizophora

Woods sold under several trade names often come from one genus. These 4 share the genus Rhizophora, so they are close relatives and frequent substitutes for each other.

1 of 4 carry a published Janka test.

WoodJankaDensity
MangleRhizophora apiculata3,965 lbf*73.4 lb/ft³
Mangle ColoradoRhizophora mangle2,760 lbf67.0 lb/ft³
Mangle hembraRhizophora mucronata2,607 lbf*60.4 lb/ft³
Rhizophora stylosaRhizophora stylosa2,607 lbf*60.4 lb/ft³