Woods sold under several trade names often come from one genus. These 5 share the genus Rhus, so they are close relatives and frequent substitutes for each other.

0 of 5 carry a published Janka test.

WoodJankaDensity
African sumacRhus lancea818 lbf*35.2 lb/ft³
Prairie sumacRhus lanceolata679 lbf*32.3 lb/ft³
Staghorn sumacRhus typhina818 lbf*35.2 lb/ft³
TavaiRhus taitensis714 lbf*33.1 lb/ft³
Winged sumacRhus copallinum818 lbf*35.2 lb/ft³