Woods sold under several trade names often come from one genus. These 2 share the genus Sabal, so they are close relatives and frequent substitutes for each other.

0 of 2 carry a published Janka test.

WoodJankaDensity
Cabbage palmettoSabal palmetto641 lbf*31.5 lb/ft³
Dwarf palmettoSabal minor1,054 lbf*39.6 lb/ft³