genus
Salix
Woods sold under several trade names often come from one genus. These 21 share the genus Salix, so they are close relatives and frequent substitutes for each other.
0 of 21 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Arroyo willowSalix lasiolepis | 791 lbf* | 34.7 lb/ft³ |
| Balsam willowSalix pyrifolia | 451 lbf* | 26.7 lb/ft³ |
| Bebb willowSalix bebbiana | 451 lbf* | 26.7 lb/ft³ |
| Black willowSalix nigra | 471 lbf* | 27.3 lb/ft³ |
| Bonpland willowSalix bonplandiana | 451 lbf* | 26.7 lb/ft³ |
| Coastal plain willowSalix caroliniana | 451 lbf* | 26.7 lb/ft³ |
| Corkscrew willowSalix matsudana | 451 lbf* | 26.7 lb/ft³ |
| Crack willowSalix fragilis | 451 lbf* | 26.7 lb/ft³ |
| Diamondleaf willowSalix planifolia | 451 lbf* | 26.7 lb/ft³ |
| Elaeagnus willowSalix elaeagnos | 451 lbf* | 26.7 lb/ft³ |
| Geyer willowSalix geyeriana | 451 lbf* | 26.7 lb/ft³ |
| Goodding's willowSalix gooddingii | 451 lbf* | 26.7 lb/ft³ |
| Peachleaf willowSalix amygdaloides | 451 lbf* | 26.7 lb/ft³ |
| Pussy willowSalix discolor | 451 lbf* | 26.7 lb/ft³ |
| Red willowSalix laevigata | 451 lbf* | 26.7 lb/ft³ |
| Salix humboldtianaSalix humboldtiana | 573 lbf* | 29.8 lb/ft³ |
| Scouler's willowSalix scouleriana | 451 lbf* | 26.7 lb/ft³ |
| Silky willowSalix sericea | 451 lbf* | 26.7 lb/ft³ |
| Sitka willowSalix sitchensis | 451 lbf* | 26.7 lb/ft³ |
| White willowSalix alba | 451 lbf* | 26.7 lb/ft³ |
| Yellow willowSalix lutea | 451 lbf* | 26.7 lb/ft³ |