genus
Sambucus
Woods sold under several trade names often come from one genus. These 2 share the genus Sambucus, so they are close relatives and frequent substitutes for each other.
0 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Common elderberrySambucus nigra | 832 lbf* | 35.5 lb/ft³ |
| Red elderberrySambucus racemosa | 672 lbf* | 32.2 lb/ft³ |