Woods sold under several trade names often come from one genus. These 5 share the genus Sapium, so they are close relatives and frequent substitutes for each other.
3 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Burra-leiteiraSapium marmieri | 324 lbf | 30.0 lb/ft³ |
| HinchahuevosSapium laurifolium | 542 lbf* | 29.1 lb/ft³ |
| LecheroSapium spp. | 700 lbf | 36.0 lb/ft³ |
| LeiteiroSapium glandulosum = Sapium aereum | 379 lbf | 32.5 lb/ft³ |
| MilktreeSapium laurocerasus | 509 lbf* | 28.2 lb/ft³ |