Wood Record

genus

Senna

Woods sold under several trade names often come from one genus. These 8 share the genus Senna, so they are close relatives and frequent substitutes for each other.

0 of 8 carry a published Janka test.

WoodJankaDensity
Argentine sennaSenna corymbosa1,309 lbf*43.8 lb/ft³
Casia amarillaSenna spectabilis1,007 lbf*38.8 lb/ft³
False sicklepodSenna multijuga791 lbf*34.7 lb/ft³
Flor de San JoseSenna atomaria1,658 lbf*48.9 lb/ft³
Gaudichauds sennaSenna gaudichaudii1,852 lbf*51.5 lb/ft³
SennaSenna septemtrionalis1,309 lbf*43.8 lb/ft³
Siamese cassiaSenna siamea1,990 lbf*53.3 lb/ft³
ValamuertoSenna pendula1,852 lbf*51.5 lb/ft³