Sideroxylon
Woods sold under several trade names often come from one genus. These 8 share the genus Sideroxylon, so they are close relatives and frequent substitutes for each other.
0 of 8 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| BreakbillSideroxylon obovatum | 2,287 lbf* | 56.9 lb/ft³ |
| Buckthorn bullySideroxylon lycioides | 1,054 lbf* | 39.6 lb/ft³ |
| False masticSideroxylon foetidissimum | 3,241 lbf* | 66.9 lb/ft³ |
| Puerto Rico bullySideroxylon portoricense | 2,692 lbf* | 61.3 lb/ft³ |
| Saffron plumSideroxylon celastrinum | 1,923 lbf* | 52.4 lb/ft³ |
| Tamaulipan ComaSideroxylon laetevirens | 1,054 lbf* | 39.6 lb/ft³ |
| Tough bullySideroxylon tenax | 1,054 lbf* | 39.6 lb/ft³ |
| Willow busticSideroxylon salicifolium | 2,867 lbf* | 63.1 lb/ft³ |