Wood Record

genus

Sloanea

Woods sold under several trade names often come from one genus. These 2 share the genus Sloanea, so they are close relatives and frequent substitutes for each other.

2 of 2 carry a published Janka test.

WoodJankaDensity
UrucuranaSloanea nitida4,057 lbf67.4 lb/ft³
UrucuranaSloanea sp.4,206 lbf59.9 lb/ft³