0 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Earleaf nightshadeSolanum mauritianum | 573 lbf* | 29.8 lb/ft³ |
| Forest nightshadeSolanum nudum | 753 lbf* | 33.9 lb/ft³ |
| Mullein nightshadeSolanum donianum | 542 lbf* | 29.1 lb/ft³ |
| PotatotreeSolanum erianthum | 679 lbf* | 32.3 lb/ft³ |