Wood Record

genus

Sophora

Woods sold under several trade names often come from one genus. These 3 share the genus Sophora, so they are close relatives and frequent substitutes for each other.

0 of 3 carry a published Janka test.

WoodJankaDensity
MamaniSophora chrysophylla2,867 lbf*63.1 lb/ft³
Mescal beanSophora secundiflora1,475 lbf*46.4 lb/ft³
Silver bushSophora tomentosa1,363 lbf*44.7 lb/ft³