Wood Record

genus

Sorbus

Woods sold under several trade names often come from one genus. These 5 share the genus Sorbus, so they are close relatives and frequent substitutes for each other.

0 of 5 carry a published Janka test.

WoodJankaDensity
American mountain-ashSorbus americana1,103 lbf*40.5 lb/ft³
European mountain-ashSorbus aucuparia1,054 lbf*39.6 lb/ft³
Greene's mountain ashSorbus scopulina1,054 lbf*39.6 lb/ft³
Northern mountain-ashSorbus decora1,054 lbf*39.6 lb/ft³
Western mountain ashSorbus sitchensis1,054 lbf*39.6 lb/ft³