Wood Record

genus

Spondias

Woods sold under several trade names often come from one genus. These 4 share the genus Spondias, so they are close relatives and frequent substitutes for each other.

1 of 4 carry a published Janka test.

WoodJankaDensity
CajáSpondias mombin = Spondias lutea359 lbf28.1 lb/ft³
Purple mombinSpondias purpurea423 lbf*26.0 lb/ft³
Spondias dulcisSpondias dulcis395 lbf*25.1 lb/ft³
TitmelSpondias pinnata321 lbf*22.8 lb/ft³