genus
Sterculia
Woods sold under several trade names often come from one genus. These 7 share the genus Sterculia, so they are close relatives and frequent substitutes for each other.
6 of 7 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AxixáSterculia apeibophylla | 686 lbf | 38.1 lb/ft³ |
| Brown SterculiaSterculia rhinopetala | 1,810 lbf | 50.0 lb/ft³ |
| ChichaSterculia apetala | 400 lbf | 25.0 lb/ft³ |
| Hazel sterculiaSterculia foetida | 875 lbf* | 36.3 lb/ft³ |
| SterculiaSterculia pruriens | 798 lbf | 37.0 lb/ft³ |
| XixáSterculia excelsa = Sterculia speciosa | 1,071 lbf | 39.4 lb/ft³ |
| Yellow SterculiaSterculia oblonga | 1,120 lbf | 48.0 lb/ft³ |