Woods sold under several trade names often come from one genus. These 2 share the genus Swietenia, so they are close relatives and frequent substitutes for each other.

1 of 2 carry a published Janka test.

WoodJankaDensity
True mahoganySwietenia macrophylla800 lbf41.0 lb/ft³
West Indian mahoganySwietenia mahagoni1,419 lbf*45.5 lb/ft³