genus
Syzygium
Woods sold under several trade names often come from one genus. These 7 share the genus Syzygium, so they are close relatives and frequent substitutes for each other.
0 of 7 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AsiSyzygium inophylloides | 2,367 lbf* | 57.7 lb/ft³ |
| Brush cherrySyzygium paniculatum | 1,598 lbf* | 48.1 lb/ft³ |
| Java plumSyzygium cumini | 1,658 lbf* | 48.9 lb/ft³ |
| Malaysian appleSyzygium malaccense | 1,007 lbf* | 38.8 lb/ft³ |
| Ohia haSyzygium sandwicense | 1,990 lbf* | 53.3 lb/ft³ |
| Sea appleSyzygium grande | 1,054 lbf* | 39.6 lb/ft³ |
| Syzygium jambosSyzygium jambos | 1,598 lbf* | 48.1 lb/ft³ |