Woods sold under several trade names often come from one genus. These 8 share the genus Tabebuia, so they are close relatives and frequent substitutes for each other.

4 of 8 carry a published Janka test.

WoodJankaDensity
IpeTabebuia spp., lapacho group3,680 lbf70.0 lb/ft³
IpêTabebuia sp1,280 lbf63.7 lb/ft³
Pink tabebuiaTabebuia pallida1,054 lbf*39.6 lb/ft³
Pink trumpet-treeTabebuia rosea1,054 lbf*39.6 lb/ft³
PrimaveraTabebuia donnell–smithii660 lbf29.0 lb/ft³
RobeTabebuia spp., roble group960 lbf40.0 lb/ft³
Roble coloradoTabebuia schumanniana1,923 lbf*52.4 lb/ft³
White cedarTabebuia heterophylla1,152 lbf*41.3 lb/ft³