genus
Tachigali
Woods sold under several trade names often come from one genus. These 7 share the genus Tachigali, so they are close relatives and frequent substitutes for each other.
7 of 7 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Pau-pongaTachigali sp. | 1,019 lbf | 36.2 lb/ft³ |
| TaxiTachigali glauca = Tachigali myrmecophila | 1,505 lbf | 43.4 lb/ft³ |
| Taxi-brancoTachigali cavipes | 818 lbf | 34.3 lb/ft³ |
| Taxi-pitombaTachigali chrysophylla =Sclerolobium chrysophyllum | 1,378 lbf | 47.7 lb/ft³ |
| Taxi-pitombaTachigali poeppigiana = Sclerolobium poeppigianum | 1,479 lbf | 50.7 lb/ft³ |
| Taxi-preto / taxiaranaTachigali paraensis = Sclerolobium paraense | 1,962 lbf | 47.3 lb/ft³ |
| Taxi-preto / ziquitaTachigali multijuga | 1,166 lbf | 40.0 lb/ft³ |