Wood Record

genus

Tamarix

Woods sold under several trade names often come from one genus. These 3 share the genus Tamarix, so they are close relatives and frequent substitutes for each other.

0 of 3 carry a published Janka test.

WoodJankaDensity
Athel tamariskTamarix aphylla1,255 lbf*43.0 lb/ft³
Five-stamen tamariskTamarix chinensis1,054 lbf*39.6 lb/ft³
SaltcedarTamarix ramosissima1,788 lbf*50.7 lb/ft³