Wood Record

genus

Taxus

Woods sold under several trade names often come from one genus. These 4 share the genus Taxus, so they are close relatives and frequent substitutes for each other.

0 of 4 carry a published Janka test.

WoodJankaDensity
European yewTaxus baccata1,009 lbf*45.5 lb/ft³
Florida yewTaxus floridana1,038 lbf*46.4 lb/ft³
Japanese yewTaxus cuspidata1,038 lbf*46.4 lb/ft³
Pacific yewTaxus brevifolia1,038 lbf*46.4 lb/ft³