genus
Terminalia
Woods sold under several trade names often come from one genus. These 14 share the genus Terminalia, so they are close relatives and frequent substitutes for each other.
7 of 14 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Cachaporra-do-gentioTerminalia cf argentea | 3,139 lbf | 60.6 lb/ft³ |
| East Indian almondTerminalia myriocarpa | 1,152 lbf* | 41.3 lb/ft³ |
| IdígboTerminalia ivorensis | 845 lbf | 32.0 lb/ft³ |
| Indian Almond WoodTerminalia catappa | 1,030 lbf* | 40.0 lb/ft³ |
| Indian LaurelTerminalia tomentosa complex | 2,220 lbf | 54.0 lb/ft³ |
| LimbaTerminalia superba | 490 lbf | 34.0 lb/ft³ |
| MaliliTerminalia richii | 1,309 lbf* | 43.8 lb/ft³ |
| Peruvian almondTerminalia oblonga | 1,788 lbf* | 50.7 lb/ft³ |
| Strand treeTerminalia litoralis | 1,203 lbf* | 42.1 lb/ft³ |
| TalieTerminalia samoensis | 1,538 lbf* | 47.3 lb/ft³ |
| TanimbucaTerminalia amazonia | 2,235 lbf | 64.1 lb/ft³ |
| Tropical almondTerminalia kaernbachii | 1,152 lbf* | 41.3 lb/ft³ |
| White BombayTerminalia procera | 1,070 lbf | 40.0 lb/ft³ |
| White ChuglamTerminalia bialata | 1,190 lbf | 43.0 lb/ft³ |