Wood Record

genus

Tetragastris

Woods sold under several trade names often come from one genus. These 3 share the genus Tetragastris, so they are close relatives and frequent substitutes for each other.

3 of 3 carry a published Janka test.

WoodJankaDensity
BarroteTetragastris panamensis2,693 lbf57.4 lb/ft³
Breu-mangaTetragastris altissima2,169 lbf58.7 lb/ft³
SaliTetragastris spp.1,970 lbf54.0 lb/ft³