Woods sold under several trade names often come from one genus. These 2 share the genus Thespesia, so they are close relatives and frequent substitutes for each other.

0 of 2 carry a published Janka test.

WoodJankaDensity
MagaThespesia grandiflora1,475 lbf*46.4 lb/ft³
Portia treeThespesia populnea1,103 lbf*40.5 lb/ft³